Download PDF

Infrastructures

Publication date: 2018-01-31
14
Publisher: MDPI

Author:

Craeye, Bart
Cockaerts, Geert ; Kara De Maeijer, Patricija

Keywords:

Science & Technology, Technology, Construction & Building Technology, Engineering, Civil, Transportation Science & Technology, Engineering, Transportation, concrete road infrastructure, superabsorbent polymers (SAPs), freeze-thaw resistance, scaling, 3509 Transportation, logistics and supply chains, 4005 Civil engineering

Abstract:

The scope of the paper is to report an investigation on durability of infrastructure concrete for roads and bridges by creating a size and shape-designed pore systems in concrete in order to improve it, especially in terms of freeze–thaw resistance. By means of this experimental laboratory study, an alternative for usage of air entrainment agents (AEA) in concrete infrastructures was found in the way of using superabsorbent polymer materials (SAPs). The effect of the addition of SAPs of different amounts and different types into fresh concrete mix was investigated, including: compressive strength tests, weight loss measurements, visual and microscopic inspections and scanning electron microscopy (SEM) analysis. The detrimental strength reduction effect was not observed. The freeze–thaw procedure was varied, using different types of de-icing salts and heating/cooling regimes. It can be concluded that an improvement of the freeze–thaw resistance of concrete infrastructure depends on the particle size and optimal amount of SAPs added into concrete mix. The addition of 0.26 wt % of dry SAPs into the fresh concrete reference mix led to the significant decrease of scaling up to 43% after 28 freeze–thaw cycles. Both dosage and particle size of the SAPs had a significant impact on the obtained results and the freeze–thaw resistance in this experimental laboratory study.