IADR, Date: 2004/03/10 - 2004/03/13, Location: Hawaii
Author:
Abstract:
Objective: The purpose of this study was to evaluate the micro-tensile bond strength (µTBS) of two adhesives at 1 hour after their application. Methods: The three-step etch&rinse adhesive Optibond FL (Kerr: O-FL) and two-step self-etch adhesive Clearfil SE (Kuraray: C-SE) were used to bond Z100 (3M Espe) to twenty mid-coronal dentin surfaces, prepared from non-carious human third molars. Half of the specimens were immediately sectioned, trimmed into a round cross-sectional shape and subjected to µTBS-testing at 1 hour after application. The remaining specimens were sectioned, trimmed and subjected to µTBS-testing after 24 hours storage in 37oC water (control). Significant differences in µTBS were determined using ANOVA and Games-Howell post-hoc test (p<0.05). Fracture analysis using stereomicroscopy was done to estimate the area percentage of ²adhesive² failure at the interface per total surface area. When the area fraction was larger than 50%, the specimen was counted as ²specimen failed adhesively² (SFA). The frequency of SFA per total specimen number was statistically analyzed using Fisher¢s exact test (p<0.05). Results: The µTBS (MPa) of O-FL at 1 hour and at 24 hours, of C-SE at 1 hour and at 24 hours were 30.0+/-9.5 and 40.9+/-13.6, 36.1+/-10.8 and 27.9+/-7.1, respectively. Statistically, O-FL at 24 hours showed a higher µTBS than O-FL at 1 hour and C-SE at 24 hours. The frequency of SFA of O-FL at 1 hour and at 24 hours, of C-SE at 1 hour and at 24 hours were 6/16, 1/19, 3/16 and 2/19, respectively. A significant difference was observed between O-FL at 1 hour and at 24 hours. Conclusions: The early 1-hour µTBS to dentin was lower than the 24-hour µTBS for OptiBond FL, but not for Clearfil SE. Differences in polymerization efficiency as well as in the resulting interfacial strength may explain such varying µTBSs.